Specific Heat Measurements on Amorphous and Nanocrystalline Al88Y5Ni5Co2
(Elsevier, 2009)
Specific heat at constant pressure, CP, was measured on amorphous and nanocrystalline Al88Y5Ni5Co2 alloys from differential scanning calorimetry experiments. Linear behavior of CP versus temperature from 323 to 423 K is ...
Artículo
Kinetic and Microstructural Studies on the Devitrification of Fe60-xCo18MnxNb6B16 Amorphous Alloys
(Elsevier, 2008)
Kinetic and microstructural studies have been performed on Fe60-xCo18MnxNb6B16 (x = 0, 2, 4) alloys by using different techniques. Isothermal and non-isothermal kinetics agree describing the nanocrystallization as a strongly ...
Artículo
The magnetocaloric effect in soft magnetic amorphous alloys
(2007)
The influence of different compositional modifications on the magnetic entropy change and refrigerant capacity of Finemet, Nanoperm, HiTperm, and bulk amorphous alloys is presented. For all the studied alloys, the field ...
Artículo
Preferential Co Partitioning to α-Fe in Nanocrystalline CoFeNbB Alloys by Mn Addition
(Elsevier, 2009)
Influence of Mn addition on the microstructure and hyperfine parameters of amorphous and nanocrystalline Co60(FeMn)18Nb6B16 alloys has been studied. Although Mn addition does not yield significant differences in crystallization ...
Artículo
Thermal and Microstructural Stability of the Soft Magnetic Fe60Co18Nb6B15Cu1 alloy
(Elsevier, 2007)
Temperature evolution of the coercivity of nanocrystalline samples of Fe60Co18Nb6B15Cu1 alloy with different crystalline fractions was measured from room temperature up to 690 K. Although room temperature coercivity increases ...
Artículo
High Temperature Coercivity of Nb-containing HITPERM Alloys: Effect of Cu Addition
(Elsevier, 2008)
Hysteresis loops of nanocrystalline samples of Fe39Co39Nb6B16 - yCuy (y = 0, 1) HITPERM-type alloys were measured from room temperature up to 773K. The alloy with Cu shows a nearly constant value of coercivity (∼ 135A/m) ...