Buscar
Mostrando ítems 1-6 de 6
Artículo
Influence of Milling Time on the Homogeneity and Magnetism of a Fe70Zr30 Partially Amorphous Alloy: Distribution of Curie Temperatures
(MDPI, 2020)
In this work, the mechanically alloyed Fe70Zr30 (at. %) composition has been used to study the influence of milling time on its homogeneity and magnetic properties. The microstructure and Fe environment results show the ...
Artículo
Kinetic and Microstructural Studies on the Devitrification of Fe60-xCo18MnxNb6B16 Amorphous Alloys
(Elsevier, 2008)
Kinetic and microstructural studies have been performed on Fe60-xCo18MnxNb6B16 (x = 0, 2, 4) alloys by using different techniques. Isothermal and non-isothermal kinetics agree describing the nanocrystallization as a strongly ...
Artículo
Extracting the composition of nanocrystals of mechanically alloyed systems using Mössbauer spectroscopy
(Elsevier, 2014)
Determining the composition at the nanoscale generally requires the use of experimental techniques such as 3D atom probe or nanoanalysis, which have limited availability, involve high economic cost and, moreover, imply ...
Artículo
Evolution of Fe environments in mechanically alloyed Fe–Nb–(B) compositions
(Elsevier, 2014)
Nanocrystalline alloys of nominal composition Fe85Nb5B10 were produced by mechanical alloying from a mixture of elemental powders. Two commercial boron structures were used: amorphous and crystalline. In addition, a third ...
Artículo
Study of the Kinetics and Products of the Devitrification Process of Mechanically Amorphized Fe70Zr30 Alloy
(Elsevier, 2020)
Devitrification of mechanically alloyed amorphous Fe70Zr30 at. % compound consists on a two-step process: amorphous → amorphous + bcc Fe + Fe2Zr → Fe2Zr + Fe23Zr6. This sequence is inferred from the evolution of the Mössbauer ...
Artículo
High Temperature Coercivity of Nb-containing HITPERM Alloys: Effect of Cu Addition
(Elsevier, 2008)
Hysteresis loops of nanocrystalline samples of Fe39Co39Nb6B16 - yCuy (y = 0, 1) HITPERM-type alloys were measured from room temperature up to 773K. The alloy with Cu shows a nearly constant value of coercivity (∼ 135A/m) ...