Compressive strength degradation in ZrB2-based ultra-high temperature ceramic composites
(Elsevier, 2011)
The high temperature compressive strength behavior of zirconium diboride (ZrB2)-silicon carbide (SiC) particulate composites containing either carbon powder or SCS-9a silicon carbide fibers was evaluated in air. Constant ...
Artículo
Artículo
Microstructure and Thermal Conductivity of Si-Al-C-O Fiber Bonded Ceramics Joined to Refractory Metals
(Elsevier, 2020)
We explore joining Si-Al-C-O fiber-bonded ceramics to Cu-clad-Mo using an Ag-Ti-Cu brazing alloy. A temperature of 900 °C and times in the range of 10–20 min are required to obtain sound joints irrespectively of the fiber ...